MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Resin Technology Group 401 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Electrically Conductive

Material Notes:
Oxy-Bond and Millenium Adhesive Systems
Engineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to match a variety of specific application parameters, including MIL-APPROVED. Custom designed bonding products and expert technical assistance are always available.

Resin Technology Group 401 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Room temperature curing, two part silver conductive epoxy.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 4.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 23.0 °C
Pot Life 90 min
 90 min
 
Descriptive Properties
ViscositySmooth Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resin Technology Group 404 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Resin Technology Group 405 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Resin Technology Group 408 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Resin Technology Group 451 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Resin Technology Group 157-F Oxy-Bond™ Thermally Conductive Epoxy Adhesive

PRESINT14 / 65445

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.