MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Synthos ES-FM95 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Description: ES-FM series is a special kind of polyester-based thermoplastic polyurethane elastomer, which is designed for blowing film.

Features:

  • Low melting point
  • High frequency easily cut
  • Butt fusion welding
  • Excellent processing stability
  • Outstanding water-proofing and breathable
Application: Laminated film for clothing, home textile, laminated film in football, luggage, waterproof breathable film, tents, rubber boats, fabric fitting and leather etc.

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.24 g/cc0.0434 - 0.0448 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 95 - 9795 - 97ASTM D2240
Tensile Strength 34.0 - 45.0 MPa4930 - 6530 psiASTM D412
Elongation at Break >= 450 %>= 450 %ASTM D412
100% Modulus 7.00 - 14.0 MPa1020 - 2030 psiASTM D412
300% Modulus 16.0 - 23.0 MPa2320 - 3340 psiASTM D412
Tear Strength 100 - 170 kN/m571 - 970 pliASTM D624

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUNDOW155 / 320186

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.