MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
STAR Thermoplastic Alloys & Rubbers Starflex® LC 25193 Optiflex P 7012-1000 Thermoplastic Rubber  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Information provided by STAR Thermoplastic Alloys & Rubbers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 1210 sec
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 380 - 400 °F
Front Barrel Temperature 390 - 420 °F
Nozzle Temperature 400 - 420 °F
Mold Temperature 100 - 140 °F
Injection Pressure 500 - 700 psi
Back Pressure 80.0 - 150 psi
 
Descriptive Properties
ColorTranslucent
Injection RateModerate

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
STAR Thermoplastic Alloys & Rubbers Starflex® P 7007 Thermoplastic Elastomer
STAR Thermoplastic Alloys & Rubbers Starflex® P 7057-1001 Thermoplastic Elastomer
STAR Thermoplastic Alloys & Rubbers Starflex® P 7054 Thermoplastic Elastomer
STAR Thermoplastic Alloys & Rubbers Starflex® P 7045-9000 Thermoplastic Elastomer
STAR Thermoplastic Alloys & Rubbers Starflex® P 7374 Thermoplastic Elastomer

PSTAR01 / 68534

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.