MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials TPSiV® 4200-75A SR Black Silicone Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Silicone thermoplastic elastomer with good chemical resistance and excellent abrasion resistance.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccISO 1183
Spiral Flow 13.0 cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 78
@Time 3.00 sec
ISO 7619-1
Tensile Strength at Break 24.0 MPaISO 527-1/-2
Elongation at Break 560 %ISO 527-1/-2
100% Modulus 4.50 MPa
@Strain 100 %
ISO 527-1/-2
Tear Strength 72.0 kN/mnormal; ISO 34-1
 
Processing PropertiesOriginal ValueComments
Melt Temperature 205 °COptimum Injection
Mold Temperature 10.0 - 40.0 °CInjection
 25.0 °COptimum Injection
Drying Temperature 90.0 °C
@Time 10800 - 21600 sec
Recommended; Dehumidified Dryer; Injection
Moisture Content 0.030 %Injection
Back Pressure 0.700 - 1.40 MPaInjection
Vent Depth 0.00130 cmInjection
 0.00250 cmInjection
 
Descriptive Properties
ColorBlack
CompatibilityPolycarbonate
 Polyurethane
 Polyvinylchloride
 Styrenics
Delivery formPellets
Max. processing screw tangential speed (m/s)0.4Injection
ProcessingExtrusion
 Injection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Special characteristicsLight stabilized or stable to light
 Soft touch

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZDSX4905 / 249184

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.