MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Synfoam® HT-17 Syntactic Foam
Categories: Polymer; Thermoset

Material Notes: Pre-cast. SynFoam HT is a high performance, light weight pre-cast syntactic foam that provides the best combination of high temperature resistance and dielectric properties. SynFoam HT has a low coefficient of thermal expansion and good strength. In addition to being used for weight reduction SynFoam HT is also used in the microwave industry because of the dielectric properties which show outstanding performance over a wide frequency range up to 10 GHz. SynFoam HT is an ideal structural core material for applications that will be exposed to higher temperatures and has been used to replace honeycomb structures. SynFoam HT is chemically stable, UV resistant and does not absorb water. SynFoam HT is available as 4” x 12” x 12” fully cured blocks. The blocks may be further machined into different sizes and shapes by the end user to meet the necessary specific tolerances and requirements. Our syntactic foam is easily bonded together with the use of our syntactic adhesive to form large structures.

Information provided by Synfoam®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 15.0 - 19.0 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 950 psi
Compressive Modulus 40000 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 µm/m-°C
Glass Transition Temp, Tg 180 °C
 
Descriptive Properties
Sound Velocity (m/s)1800

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Synfoam® HT-19 Syntactic Foam
General Plastics LAST-A-FOAM® FR-4718 Foam
General Plastics LAST-A-FOAM® FR-4625 Foam
3A Composites Core Materials AIREX® C70.250 Universal Structural Foam

PSYNF014 / 192889

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.