MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
ConocoPhillips Conoco® El Mar® Geo Low Ash Oil, SAE Viscosity Grade 40  (discontinued **)
Categories: Fluid; Lubricant

Material Notes: Conoco® El Mar GEO Oil is a high-quality, non-detergent, ashless gas engine oil designed primarily for use in Ajax 2-stroke cycle natural gas engines. The SAE 15W-40 viscosity grade meets the low-temperature viscosity requirements of Ajax engines where cold starts and frequent start/stop cycles may be encountered. El Mar GEO Oil is formulated to provide excellent resistance tooxidation and nitration, protect against ring and liner wear, minimize the formation of sludge and piston deposits for excellent engine cleanliness, and protect against corrosion. The absence of ash-forming additives results in clean intake ports to help maintain peak engine performance, and also helps extend spark plug life in spark-ignited gas engines. This oil is formulated to meet the requirements of gas engines equipped with exhaust after treatment devices.

Applications:

  • 2 Cooper-Ajax 2-stroke cycle natural gas engines (SAE 15W-40)
  • Older, horizontal-type 2-stroke cycle natural gas engines, such as those manufactured by Cooper-Bessemer and Worthington (SAE 30/40)
El Mar GEO Oil is approved for use under the following OEM specification:
  • DuPont Specification A4V4
Features/Benefit:
  • Ashless formulation helps minimize port deposits
  • Protects against sludge and varnish formation
  • Excellent resistance to oxidation and nitration
  • Protects against scuffing and wear
  • Protects against rust and corrosion
  • Excellent water-separating properties
  • Low carbon-forming tendency
  • Compatible with emissions system catalysts
  • Does not contain any bright stock, which can cause harmful carbon deposits

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012. The Conoco brand name is no longer in use on their lubricants, but these products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.885 g/cc
@Temperature 15.6 °C
Density 7.37 lb/gal
Viscosity Measurement 91Viscosity Index
Kinematic Viscosity at 40°C (104°F) 133 cSt
Kinematic Viscosity at 100°C (212°F) 13.1 cSt
Ash <= 0.010 %Sulfated Ash; ASTM D874
ASTM Color 3.0ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.14ASTM D974
 
Thermal PropertiesOriginal ValueComments
Pour Point -11.0 °F
Flash Point 536 °FCOC
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.0030 %
 
Descriptive Properties
Carbon Reside0.05%ASTM D524

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON253 / 75290

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.