In binding materials for production of wood laminate, base of glues for wood materials, for impregnation of paper during production of synthetic veneer sheet, production of varnish, production of rods and forms in the metallurgical industry. Mixing of resin with water in ratio of 2:1-1:10 where there is coagulation in volume. |