MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polytek Poly-Optic® 1410 Low Viscosity, Polyurethane Casting Resins
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Description: Poly-Optic® 14-Series Casting Resins are two-part, polyurethane systems formulated specifically for applications where optical clarity is required. Castings are clear like water; however, PolyColor dyes can be added to obtain clear, colored castings. Poly-Optic systems, with low viscosities and long pot-lives, provide for easy mixing, excellent detail penetration, and easy degassing, through vacuum or pressure casting techniques, for bubble-free castings.

Product Line Features:

  • Crystal clear
  • Reproduces fine detail
  • Can be machined, drilled and sanded
  • Tough and hard, but not brittle
  • Long working time
  • Low shrinkage upon cure

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.07 g/cc1.07 g/cc
Viscosity 700 cP700 cPInitial Mixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Tensile Strength 31.48 MPa4566 psi
Elongation at Break 27 %27 %
Modulus of Elasticity 0.667 GPa96.8 ksi
Flexural Strength 33.74 MPa
@Strain 5.0 %
4893 psi
@Strain 5.0 %
Flexural Modulus 0.993934 GPa144.158 ksi
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 37.8 °C100 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Thickness 25.4 mm
2.00 hour
@Thickness 1.00 in
Demold Time
Pot Life 15.0 min15.0 min
 
Descriptive Properties
Cured ColorWater Clear
Maximum Exotherm265°F
Mix Ratio By Weight3A:2B
Specific Volume25.8 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTK5076 / 251068

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.