PPE-PA66 Alloy. High flowability. Lemalloy provides well-balanced mechanical, electrical, and thermal properties. In addition, Lemalloy boasts the lowest specific gravity among engineering plastics. Equipped with the above features, Lemalloy meets market requirements for compactness, high performance, and flame retardance. Stable rigidity, impact strength and fatigue resistance through a wide range of temperatures. Excellent insulation properties, low dielectric constant and low dielectric dissipation factor. Excellent dimensional stability with low water absorption. Excellent heat stability. Low specific gravity. Excellent moldability and low shrinkage rate for quality precision parts. Excellent processability; good mold release, easy flow properties and a wide range of stock temperatures.Information provided by Mitsubishi Engineering Plastics Corporation. |