MDI blend with low viscosity developed as isocyanate component of flexible polyurethane foams used in automotive headrests, armrests and acoustic insulation components. Uses: Flexible foams: Automotive headrests, Automotive armrests Information provided by BorsodChem Rt. |
Methyl Diphenyl Diisocyanate |