MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Americas Styrenics STYRON A-TECH® 1260 High Impact Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Product Characteristics
  • Good Environmental Stress Crack Resistance (ESCR)
  • Good practical toughness
  • Deep draw thermoforming capable
  • Good low temperature impact
  • Food Contact Compliant

Typical Applications

  • Packaging for foods such as yogurt, sour cream, delicatessen salads and gravy
  • Containers and lids
  • Cold temperature packaging
  • Portion dairy containers

Information provided by AmericasStyrenics LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 in/inASTM D955
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110ASTM D785
Tensile Strength at Break 3300 psiASTM D638
Tensile Strength 2700 psiASTM D638
Elongation at Break 60 %ASTM D638
Tensile Modulus 190 ksiASTM D638
Flexural Strength 5400 psiASTM D790
Flexural Modulus 230 ksiASTM D790
Izod Impact, Notched 2.20 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 183 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 159 °FASTM D648
Vicat Softening Point 220 °FASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Americas Styrenics EA6740 High Impact Polystyrene
Americas Styrenics STYRON® EA6740 High Impact Polystyrene
Americas Styrenics STYRON® 478 High Impact Polystyrene
Americas Styrenics STYRON® 487 High Impact Polystyrene
Chevron Phillips EC6600 HIPS - High Impact Polystyrene

PAMERI932 / 131199

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.