MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics FastDoor™ XL Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Thermal Ceramics offers another innovation to our fire rated enclosure line, the FastDoor duct access system. The FastDoor system is comprised of a UL1978 tested and listed duct access door and an ASTM E2336 tested and listed enclosure cover plate. The duct access door is tested to be grease and fire tight when immersed in a simulated grease pan fire per UL1978. The access door is Union made and under UL follow-up inspection to ensure the finest quality. An included and ready to install insulated cover plate is compatible with FireMaster FastWrap XL and Pyroscat Duct Wrap XL installation on grease or air ducts, and is the only single layer door enclosure system available. This single layer of insulation is only 1-1/2 inches thick and provides zero clearance to adjacent combustibles and 2-hour rating per the stringent ASTM E2336 grease duct enclosure standard. The FastDoor system provides for fast and simple installation surpassing the requirements of NFPA 96 and the International Mechanical Code.

Information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF70178 / 203475

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.