MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daikin DAI-EL G-962 Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: DAI-EL G-962 is a fluoroelastomer which provides excellent mechanical properties and resistance to steam and acids with good low temperature flexibility.

Introduction: DAI-EL G-962 is a peroxide curable terpolymer of vinylidene fluoride, tetrafluoroethylene and hexafluoropropylene which is suitable for injection molding; It provides excellent mechanical properties and resistance to steam and acids and a good balance of chemical resistance and low temperature flexibility.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.83 g/ccASTM D792
Mooney Viscosity 27.0
@Temperature 121 °C
ML1+10; ASTM D1646
 47.0
@Temperature 100 °C
ML1+10; ASTM D1646
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65.0peak; ASTM D2240
 63.0
@Time 3.00 sec
ASTM D2240
Tensile Strength 18.0 MPaASTM D412
Elongation at Break 280 %ASTM D412
100% Modulus 2.60 MPa
@Strain 100 %
ASTM D412
Compression Set 17.0 %
@Temperature 200 °C,
Time 252000 sec
25% compression
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -19.0 °CLow Temperature Retraction (TR10); ASTM D1329
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 67.0 %
 
Descriptive Properties
AppearanceTranslucent to pale pink

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDAIK9669 / 327109

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.