MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aperam N48 Cold Rolled Strip
Categories: Metal; Ferrous Metal

Material Notes: N48 is an iron-nickel controlled expansion alloy suitable to soft glass sealing, with optimal chemical composition to obtain hermetic seals. Typical applications are hermetic feed throughs and electron gun components.

International standards: ASTM F30 - DIN 17745 - W 1.3922 - A54-301

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 140Annealed
 220Hard Temper
Tensile Strength, Ultimate 540 MPaAnnealed
 740 MPaHard Temper
Tensile Strength, Yield 270 MPaAnnealed
 710 MPaHard Temper
Elongation at Break 5.0 %Hard Temper
 30 %Annealed
Tensile Modulus 160000 MPaYoung's, Annealed
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000050 ohm-cm
Curie Temperature 450 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.20 - 9.20 µm/m-°C
@Temperature 30.0 - 400 °C
 9.60 - 10.3 µm/m-°C
@Temperature 30.0 - 550 °C
Specific Heat Capacity 0.500 J/g-°C
Thermal Conductivity 16.0 W/m-K
Melting Point 1425 °C
 
Component Elements PropertiesOriginal ValueComments
Iron, Fe 52 %
Nickel, Ni 48 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy
Aperam N42 Cold Rolled Strip
Special Metals NILO® Alloy 42 Controlled-Expansion Alloy
Alliance N-42 Neodymium Iron Boron Magnetic Material
Alliance N-40M Neodymium Iron Boron Magnetic Material

NPERA043 / 194832

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.