MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® Fibrelam® Grade 12 Panels for Aircraft Flooring
Categories: Other Engineering Material

Material Notes: Fibrelam® structural sandwich panels have been in service since 1973 and are currently approved for flooring by major aircraft manufacturers and airlines worldwide. These extensively flight-proven panels offer outstanding mechanical and physical properties, can be easily cut and machined on equipment normally found in airline maintenance shops, and are easy to install.

Information provided by Hexcel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Burn Length (mm)56BSS 7230; Flammability: 60 Second Vertical Ignition
Drip Extinguish Time (sec)0BSS 7230; Flammability: 60 Second Vertical Ignition
Glow Time (sec)0BSS 7230; Flammability: 45 Degree Test
Impact Resistance (N-m)9.9BMS 4-17
In-Plane Shear (N/mm)175BMS 4-17
Insert Shear (N)5350BMS 4-17
Long Beam Bending Deflection (mm)8.9MIL-STD-401B; At 445N (100lb)
Long Beam Bending Load (N)3070BSS 7250 Humidity; Humidity Resistance Load (100% at 60°C (140°F) for 30 days)
 3540MIL-STD-401B; Core Ribbon, Transverse
Panel Shear Strength (N)5060MIL-STD-401B 3 point loading; Core Ribbon, Transverse
Sandwich Peel (N/76 mm)420MIL-STD-401B; Core Ribbon, Transverse
Self-Extinguish Time (sec)1BSS 7230; Flammability: 45 Degree Test
 8BSS 7230; Flammability: 60 Second Vertical Ignition
Stabilized Core Compression (N/mm2)25.8MIL-STD-401B
Warpage (mm/m), max0.8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® Fibrelam® Grade 1 Panels for Aircraft Flooring
Hexcel® Fibrelam® 5000 Grade 1/3/3 Panels for Aircraft Flooring
Hexcel® Fibrelam® Grade 5 Panels for Aircraft Flooring
Hexcel® Fibrelam® Grade 15 Panels for Aircraft Flooring
Hexcel® Fibrelam® Grade 1-3/3 Panels for Aircraft Flooring

PHEXC687 / 101306

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.