MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay RHODAFAC® HA-70 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Identification: POLYOXYETHYLENE PHENYL ESTER PHOSPHATE ACID FORM

CAS: 39464 – 70 – 5

Solublility: Readily soluble in water, ketones, alcohols and glycol ether solvents. Soluble in strong caustic solutions. Insoluble in hydrocarbon and halogenated solvents.

Available in: Asia Pacific, Europe and Latin America

Applications: Hydrotropic agent. Metal working: extreme-pressure additive for the formulation of soluble oils, synthetic and semi-synthetic fluids, cleaning fluids. This product is non-foaming.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
pH 2.22.25% aq. Sol.
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 245 - 270245 - 270[mg KOH/g]; RPG44
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 28 - 32 %28 - 32 %RPG16
 
Descriptive Properties
AppearancePale yellow liquid
Cloud point>100°C1% in 25% NAOH
Ionic ChargeAnionic
Setting point<0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODAFAC® ARB/90 Surfactant
Solvay RHODAFAC® LO/529-E Surfactant
Solvay RHODAFAC® MB Surfactant
Solvay RHODAFAC® PE-510 Surfactant
Solvay RHODAFAC® RE-610 Surfactant

WRHOD353 / 137584

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.