MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sipchem Sahara C 060CG Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Description: SAHARA C 060CG is a polypropylene impact copolymer suitable for production of beverage closures for both compression and injection molding fabrications. This product is offering a good balance between stiffness and impact strength. This product is nucleated and additives with slip and antistatic agent. It also could be used in other injection molding applications such as houseware and medium size containers.

Product Characteristics:
Commercial Status: Active.
Processing Method: Injection Molding, Compression Molding
Typical applications: Caps & Closures, Houseware and Toys.

Information provided by Sahara International Petrochemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO1183-1
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 32.0 MPa4640 psiISO 527-1, -2
Elongation at Break >= 50 %>= 50 %ISO 527-1, -2
Elongation at Yield 6.5 %6.5 %ISO 527-1, -2
Tensile Modulus 1.65 GPa239 ksiISO 527-1, -2
Flexural Modulus 1.703 GPa247.0 ksiISO 178
Izod Impact, Notched 0.0690 J/cm0.129 ft-lb/inISO 180
Charpy Impact, Notched  0.240 J/cm²
@Temperature -20.0 °C
1.14 ft-lb/in²
@Temperature -4.00 °F
Type 1, Edgewise; ISO 179
 0.380 J/cm²
@Temperature 0.000 °C
1.81 ft-lb/in²
@Temperature 32.0 °F
Type 1, Edgewise; ISO 179
 0.820 J/cm²
@Temperature 23.0 °C
3.90 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C225 °Funannealed; ISO 75B-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C136 °Funannealed; ISO 75B-1, -2
Vicat Softening Point 81.0 °C178 °FB50; ISO 306
 153 °C307 °FA50; ISO 306
 
Processing PropertiesMetricEnglishComments
Processing Temperature 210 - 250 °C410 - 482 °FBarrel temperature range

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIPCH030 / 285343

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.