LE4201EHV is a crosslinkable natural polyethylene compound, specially designed for insulation applications. LE4201EHV is intended for insulation of XLPE extra high voltage cables with rated voltages above 220kV. LE4201EHV meets these applicable requirements when processed using sound extrusion practice and testing procedure: IEC 60840; IEC 62067; and ANSI/ICEA 108-720-2004. Former trade name for this product was Superclean™. Information provided by Borealis AG |