MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ConocoPhillips Hydroclear® El Mar® Low Ash Heavy Duty SAE 40
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear El Mar Low Ash Heavy Duty is a high-quality low ash natural gas engine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear El Mar Low Ash Heavy Duty is specially formulated with proprietary additive chemistry to meet the requirements of naturally aspirated and moderately turbocharged, four-cycle, low- to medium-speed gas engines. Hydroclear El Mar Low Ash Heavy Duty has demonstrated successful performance results in small light-duty gas engines manufactured by Caterpillar and Waukesha.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.872 g/cc0.0315 lb/in³
Viscosity Measurement 101101Viscosity Index
Saybolt Viscosity at 100°F 659 SUS659 SUS
Saybolt Viscosity at 210°F 73 SUS73 SUS
Kinematic Viscosity at 40°C (104°F) 126 cSt126 cSt
Kinematic Viscosity at 100°C (212°F) 13.4 cSt13.4 cSt
Ash 0.46 %0.46 %Sulfated Ash
ASTM Color 2.02.0
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 1.11.1ASTM D974
Total Base Number 3.83.8
 
Thermal PropertiesMetricEnglishComments
Pour Point -34.4 °C-30.0 °F
Flash Point 268 °C515 °F
 
Descriptive Properties
Carbon Residue0.5 wt. %
Phosphorus270 ppm
Zinc310 ppm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON270 / 75307

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.