MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Honeywell HLT3500 Thermally Conductive Gel
Categories: Other Engineering Material

Material Notes: Benefits And Features:
  • Low contact resistance
  • Easy to dispense and rework
  • High compressibility for low stress applications
  • Long-term reliability
  • Less oil separation
  • No pump out and cracking
Overview: Honeywell HLT2000 and HLT3500 are two-part, dispensable thermally conductive gel, which offer long-term reliability and superior softness. The enhanced bonding force between the polymer base and the filler largely improves the thermally conductive gel oil separation issue in storage. Prior to curing, the material maintains good thixotropic characteristics and low viscosity to be easily dispensed. The product can be cured in short time after two-component mixing at room temperature. The high compressibility minimizes thermal resistance at interfaces, while maintaining excellent performance during reliability testing.

Typical Applications:

  • Consumer electronics
  • Telecommunications equipment
  • Automotive electronics
  • Memory & power modules

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.20 g/ccASTM D792
Brookfield Viscosity 300000 - 450000 cP#7 spindle, 10rpm; ASTM D2196
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 50ASTM D2240
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 3.50 W/m-KASTM D5470
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Temperature 100 °C
Shelf Life 6.00 Month
 
Descriptive Properties
ColorBluePart B
 WhitePart A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHONWL6001 / 255331

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.