MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trelleborg Emerson & Cuming Eccobond® C429-2 One-Component Silver Filled Electrically Conductive Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, Electrically Conductive

Material Notes: Emerson & Cuming C429-2 Eccobond® One-Component Silver Filled Electrically Conductive Epoxy Adhesive
One component, high strength, moderate cost, silver filled, electrically conductive, epoxy adhesive. Excellent adhesion and long term durability. Designed for use in miniature lamp bonding. Bonding Type: Epoxy

The Eccobond® product line is now a part of Henkel; this specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.20 g/cc
Viscosity 2.50e+6 cP
@Temperature 25.0 °C
Mixed
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 2000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.20 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 155 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.0833 hour
@Temperature 180 °C
 0.500 hour
@Temperature 150 °C
 1.50 hour
@Temperature 125 °C
 
Descriptive Properties
ColorSilver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Stycast® 1269A Two-Component Easy Mix Ratio Encapsulant
Trelleborg Emerson & Cuming Eccobond® 56C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive
Trelleborg Emerson & Cuming Eccobond® 57C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive
Trelleborg Emerson & Cuming Eccobond® 64C Two-Component Nickel Filled Electrically Conductive Epoxy Adhesive
Trelleborg Emerson & Cuming Eccobond® 83C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive

PEMERS56 / 35748

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.