MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

3M Scotchcal™ IJ5000 Reflective Graphic Film'
Categories: Polymer; Film

Material Notes: 6-mil, enclosed lens, retroflective, flexible films; Pressure-sensitive adhesive; Permanent; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Version for screen printing, inkjet printing, and electrostatic imaging; Designed for excellent cutting and weeding with computer sign cutting equipment; For vertical, flat without rivets surfaces; Unprocessed film resists fuel vapor or occasional spills

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 152 microns6.00 milwith adhesive
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.456 kN/m2.60 pliAdhesion to Painted aluminum panels
 0.649 kN/m3.70 pliAdhesion to FRP
 0.841 kN/m4.80 pliAdhesion to Aluminum
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 29.0 °C50.0 - 84.2 °FApplication Temp; Air and substrate, for flat surfaces without rivets
 13.0 - 29.0 °C55.4 - 84.2 °FApplication Temp; Air and substrate, for flat surfaces with rivets
 10.0 - 38.0 °C50.0 - 100 °FApplication Temp; Dry, flat surfaces without rivets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35083 / 169830

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.