MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex TEKRON® 4300-D88A Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes:

Information provided by Teknor Apex Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.880 - 0.920 g/ccASTM D792
Melt Density 0.785 g/cc
@Temperature >=125 °C
Linear Mold Shrinkage, Flow 0.0090 cm/cmat 80°C for 30 min.
 0.0090 cm/cm
 0.012 cm/cmat 93°C for 30 min.
Linear Mold Shrinkage, Transverse 0.0090 cm/cmat 80°C for 30 min.
 0.010 cm/cm
 0.013 cm/cmat 93°C for 30 min.
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 30 - 3610 second delay; ASTM D2240
Tensile Strength, Yield 1151 psi94% Retention; Air Over Aged 1000 hrs at 90°C
 1175 psi96% Retention; Air Over Aged 400 hrs at 107°C
 1224 psiASTM D412
 1280 psi104.6% Retention; Air Over Aged 1008 hrs at 100°C, Perpendicular
 1322 psi108% Retention; Air Over Aged 1008 hrs at 100°C, Parallel
Elongation at Break 427.5 %75% Retention; Air Over Aged 400 hrs at 107°C
 438.9 %77% Retention; Air Over Aged 1000 hrs at 90°C
 467.97 %82.1% Retention; Air Over Aged 1008 hrs at 100°C, Perpendicular
 526.68 %92.4% Retention; Air Over Aged 1008 hrs at 100°C, Parallel
 570 %ASTM D412
Flexural Modulus 20000 psiASTM D790
Tear Strength 350 pliDie C; ASTM D1004
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 2.586 J/g-°C
Thermal Conductivity 0.159 W/m-K
@Temperature 205 °C
Melting Point 125 °CNo Flow Temp
Brittleness Temperature <= -60.0 °CASTM D746
Flame Spread 1.00 in/minPass: Burn Rate- Max 100; FMVSS 302
 
Descriptive Properties
Fogging72, 6 hours at 95°C. (SAE-J1756)
Weight Change-0.5%;Air Over Aged 400 hrs at 107°C
 -0.7%; Air Over Aged 1000 hrs at 90°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ELASTO UK Dryflex® 660900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Natural
BASF Capron® BG50XFI Impact Modified Nylon 6 (Dry)
Lithium Metal, UNS L06990
Teknor Apex Monprene® MP 1304 Thermoplastic Elastomer
Teknor Apex Monprene® MP 1644 Thermoplastic Elastomer

PTEKNO299 / 70042

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.