MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Kane TIGERLAC™ 5050 Chlorine-Free Shellac
Categories: Other Engineering Material

Material Notes: TIGERLAC™ 5050 CHLORINE-FREE is a dewaxed, bleached shellac and has been prepared to be used in applications historically reserved for dewaxed flaked shellac. It is soluble in different media yielding transparent, light-colored solutions. Ready for use solutions of this natural FDA compliant and biodegradable resin are available.

Major Applications: Wood coatings and glazes, flexographic printing inks, hat proofing, hair sprays, mold-release agents, leather finishing, fruit coatings, raw material for shellac special products

Information provided by Kane International Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesOriginal ValueComments
Acid Value 65 - 80
 
Thermal PropertiesOriginal ValueComments
Melting Point 60.0 - 70.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature <=20.0 °C
 
Descriptive Properties
AppearancePale Yellow Granules/Powder
Color2 – 2 ½Index Lovibond, (20% Ethanol)
KosherO.U. - Parve
Loss on drying< 2%
Wax content< 0.2%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKKANE001 / 295534

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.