MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Entec Ezprene® 9565A PA TPV
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Product Description: 65 Shore A TPE (Thermoplastic Vulcanizate) boundable to nylon. Available in black, natural for injection molding applications with long flow lengths or requires highly cosmetic surface. This soft, easy to color material is non-hydroscopic and offers excellent chemical resistance and physical properties. EZPrene is polyolefin based and is 100% recyclable.

Availability: North America

Features: Chemical Resistant; Fatigue Resistant; Good Adhesion; Good Colorability; Low to No Water Absorption; Ozone Resistant; Recyclable Material; Soft; UV Resistant

Appearance: Black; Natural Color

Processing Method: Injection Molding

Information provided by Entec Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.942 g/cc0.0340 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  65
@Time 5.00 sec
65
@Time 0.00139 hour
Extruded; ASTM D2240
 68
@Time 5.00 sec
68
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 4.00 MPa580 psiASTM D412
Tensile Stress 1.00 MPa
@Strain 100 %
145 psi
@Strain 100 %
ASTM D412
Elongation at Break 590 %590 %ASTM D412
Tear Strength 18.1 kN/m103 pliASTM D624
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -70.0 °C-94.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 191 - 204 °C375 - 400 °F
Middle Barrel Temperature 196 - 210 °C385 - 410 °F
Front Barrel Temperature 196 - 210 °C385 - 410 °F
Nozzle Temperature 210 - 221 °C410 - 430 °F
Melt Temperature 199 - 221 °C390 - 430 °F
Mold Temperature 23.9 - 51.7 °C75.0 - 125 °F
Drying Temperature 82.2 °C180 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour
Injection Pressure 5.17 - 8.96 MPa750 - 1300 psi
Cushion 0.508 - 1.27 cm0.200 - 0.500 in
Screw Speed 50 - 200 rpm50 - 200 rpm
 
Descriptive Properties
Dynamic Service Temperature257°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENTB679 / 311372

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.