MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt POLYCOR® 224 X Series Clear Gel Coat
Categories: Polymer; Thermoset

Material Notes: The 224X series clear gelcoats are enamel like coatings developed for the composites and fiberglass industry. These gelcoats are used as an enamel coating, similar to paint and are often used as a translucent coating. The 224X series gelcoat can also be used to protect the laminate against U.V. rays. 224X series gel coats are sag resistant and have a fast curing system. This coating system is ready to spray, requiring only the proper addition of an appropriate methyl ethyl ketone peroxide to cure.
  • Formulated for spray and roll application.
  • Fast gel time and cure time that provide a good cure.
  • Require only the addition of a proper amount of MEKP to cure.
  • Resistant to thermal change and weathering
For parts in contact with water, (severe conditions) an ISO/NPG base gelcoat for marine applications is recommended. Parts that have to be assembled should be sanded and cleaned, to obtain a good adherence.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 2000 - 2600 cP2000 - 2600 cPRVF #4 Spindle @ 20 rpm
 
Processing PropertiesMetricEnglishComments
Cure Time 45.0 - 60.0 min
@Temperature 25.0 °C
0.750 - 1.00 hour
@Temperature 77.0 °F
Lay-up Time; tested @ 1,8% Norox MEKP 925 @ 25°C
Gel Time 6.00 - 12.0 min6.00 - 12.0 minat 1.8% MEKP
 
Descriptive Properties
Sag ResistanceGood at 20 mils
Thixotropic Index<6.52/20 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9260 / 231855

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.