MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Resin Technology Group UV-S-2051 High Impact, UV Curable Plastic Bonder
Categories: Polymer; Adhesive; Thermoset

Material Notes: UV S-2051 is a general purpose, fast cure response, high thermal-shock resistant, UV curing adhesive designed for use in a variety of applications including chip bonding, laminating, tacking, and sealing. It’s rubber modification provides low cure shrinkage and high-impact resistant bonds. UV S-2051 has excellent adhesion to PVC, polycarbonate, polyurethane, flexible PCB, ceramics, glass, FR4 and other plastics.

Applications:

Automotive underhood, head lamps, connector sealing, coil terminating, transducer mountings, potting switches, chip bonding, hybrid modules, potting.

Processing:

UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometers

Recommended Aurora UV light sources:

  • Aurora 455-S 5x5 High Intensity Flood
  • Aurora 461-S 1x6 High Intensity Beam
  • Aurora 100-S Spot Light Guide

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 2500 cP
@Temperature 25.0 °C
Uncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 84Cured
Hardness, Shore D 85Cured
Elongation at Break 200 %Cured
Shear Strength 2000 psiTensile
Peel Strength 30.0 pliGiven in psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 400 V/milCured
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °CCured
Minimum Service Temperature, Air -50.0 °CCured
Flash Point >= 200 °FUncured
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 80 %Mfr. Specifies clear but does not quantify
 
Descriptive Properties
ColorClear
CompositionModified Acrylic Resin
ToxicityLow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond UV15DC80 One Component, UV and Heat Curable Epoxy System
Resin Technology Group UV-412 Medium Viscosity, High Clarity, UV Curable Adhesive
Resin Technology Group UV-408 Low-Viscosity, High Clarity, UV Curable Adhesive
Resin Technology Group EN 239-2 Millennium™ UV Curable Adhesive
Resin Technology Group DPE111798-1 UV Curable Adhesive

PRESINT646 / 65530

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.