(Viewing data as-entered.
Click here
to return)
NOVA Chemicals EPS 34RCLV Expandable Polystyrene Resin
Categories:
Polymer
;
Thermoplastic
;
Polystyrene (PS)
;
Expanded Polystyrene (EPS)
Material Notes:
Applications
High Strength/High Density > 1.5pcf Packaging and Produce Boxes
Information provided by NOVA Chemicals
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
>=
1.40
lb/ft³
Batch Expansion
Descriptive Properties
Mean Unexpanded Bead Size (mm)
0.5
Targeted Pentane Content (wt%)
3.6
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
NOVA Chemicals ARCEL® 730B Expanded Polyethylene/Styrenic Polymer
BASF Styropor® P 326 C Expandable Polystyrene
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding
PNOV837 / 108889
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.