MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite RX® 1-520 Diallyl Ortho-Phthalate Molding Compound
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled

Material Notes: RX® 1-520 is a short glass fiber reinforced, non-flame retardant, diallyl ortho-phthalate molding compound, which meets the requirements of ASTM D5948 Type SDG.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.83 g/ccASTM D792
Apparent Bulk Density 0.750 g/ccASTM D1895
Water Absorption 0.25 %
@Time 173000 sec
ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 76.0 MPaASTM D638
Flexural Strength 124 MPaASTM D790
Flexural Modulus 12.4 GPaASTM D790
Compressive Strength 150 MPaASTM D695
Izod Impact, Notched 37.0 J/mASTM D256A
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.5
@Frequency 1e+6 Hz
wet; ASTM D150
Dielectric Strength 12.2 kV/mm
@Frequency 60 Hz
SS, wet; ASTM D149
Dissipation Factor 0.016
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance 130 secASTM D495
Track Resistance >= 600 secASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µm/m-°CASTM E831
Thermal Conductivity 0.280 W/m-KASTM C518
Maximum Service Temperature, Air 130 °CUL 746B Temperature Index
Deflection Temperature at 1.8 MPa (264 psi) 205 °CAs Molded; ASTM D648A
Oxygen Index 26 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PSM Industries Pacific Sintered Metals FCC-214-S High Carbon Copper Steel Powdered Metal (MPIF FC-0208-50)
PSM Industries Pacific Sintered Metals FCC-200-P High Carbon Copper Steel Powdered Metal (MPIF FC-0505-40)
PSM Industries Pacific Sintered Metals FCC-214-S(HT) High Carbon Copper Steel Powdered Metal (MPIF FC-0208-80HT)
Cosmic Plastics D33 Short Glass Fiber Filled Diallyl Iso-Phthalate Molding Compound
Cosmic Plastics D72/6120F Short Glass Fiber Filled Diallyl Iso-Phthalate Molding Compound

PSUMIT739 / 194544

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.