MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Nilit FRIANYL A63 CV-CU 0550 Nylon 6.6 for injection molding, 5% carbon fiber reinforced, 50% copper filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Nylon 6.6 for injection molding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.03 g/cc0.0733 lb/in³ISO 1183
Water Absorption 0.50 - 1.0 %0.50 - 1.0 %ISO 62
Water Absorption at Saturation 1.0 - 2.0 %1.0 - 2.0 %ISO 62
Viscosity Measurement 145145Viscosity index; ISO 307
Linear Mold Shrinkage 0.0030 - 0.010 cm/cm0.0030 - 0.010 in/inFRISETTA Test Method
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 155 MPa22500 psiISO 2039-1
Tensile Strength at Break 112 MPa16200 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Tensile Modulus 6.80 GPa986 ksiISO 527
Flexural Strength 165 MPa23900 psiISO 178
Flexural Modulus 7.05 GPa1020 ksiISO 178
Charpy Impact Unnotched 2.30 J/cm²10.9 ft-lb/in²DIN 53453
 3.00 J/cm²14.3 ft-lb/in²ISO 179/1eU
 2.20 J/cm²
@Temperature -40.0 °C
10.5 ft-lb/in²
@Temperature -40.0 °F
DIN 53453
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eA
 0.800 J/cm²3.81 ft-lb/in²DIN 53453
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 ohm-cm10000 ohm-cmIEC 93
 
Thermal PropertiesMetricEnglishComments
Melting Point 256 °C493 °FISO 3146 DSC
Maximum Service Temperature, Air 160 °C320 °FContinuous; FRISETTA Test Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient OnForce™ LFT NN-30 LCF/000 Natural Nylon 66 with 30% Long Carbon Fiber
Celanese Nilit FRIANYL A63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced
Avient OnForce™ LFT NN-40 LGF/000 Natural Nylon 66 with 40% Long Glass Fiber
Avient Lubri-Tech™ NN-20CF/15T Nylon 6/6, Carbon Fiber Reinforced, PTFE Lubricated
Avient Lubri-Tech™ NL-30CF/10T-2S Nylon 6/12, Carbon Fiber Reinforced, PTFE Lubricated

PFRI010 / 38931

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.