MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Röchling SUSTAMID® 6G Blue PA 6G/ Cast Nylon Blue
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes:

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Water Absorption 1.0 %
@Time 86400 sec
1.0 %
@Time 24.0 hour
ASTM D570
Water Absorption at Saturation 8.5 %8.5 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8585ASTM D785
Hardness, Rockwell R 115115ASTM D785
Hardness, Shore D 7878ASTM D2240
Tensile Strength, Yield 82.7 MPa12000 psiASTM D638
Elongation at Break 25 %25 %ASTM D638
Tensile Modulus 2.76 GPa400 ksiASTM D638
Flexural Strength 103 MPa15000 psiASTM D790
Flexural Modulus 2.90 GPa420 ksiASTM D790
Compressive Strength 107 MPa15500 psiASTM D695
Shear Strength 72.4 MPa10500 psiASTM D732
Izod Impact, Notched 0.320 J/cm0.600 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.220.22
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+13 ohm>= 1.00e+13 ohmASTM D257
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 81.0 µm/m-°C45.0 µin/in-°FASTM D696
Thermal Conductivity 0.245 W/m-K1.70 BTU-in/hr-ft²-°F
Melting Point 232 °C450 °F
Maximum Service Temperature, Air 110 °C230 °F
Deflection Temperature at 0.46 MPa (66 psi) 188 °C370 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C195 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Compliance PropertiesMetricEnglishComments
FDA NoNo
NSF NoNo
USDA NoNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling SUSTAMID® 6G PA 6G/ Cast Nylon
GEHR Plastics PA 6.6 Nylon 6.6, Dry

PROCH9040 / 232743

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.