MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Copper-Nickel-Phosphorus-Tellurium alloy, UNS C19100, M10 Temper, Forgings
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Hot Forged - Air Cooled

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding; Poor Suitability – Spot Weld, Seam Weld, Butt Weld

Common Fabrication Processes: Forming and Bending; Heading and Upsetting; Hot Forging and Pressing; Roll Threading and Knurling; Shearing; Swaging

Typical uses: Components; Connectors; Bolts; Nuts; Turn buckle Barrels; Bushings; Forgings; Gears; Pinions; Screw Machine Parts; Tie Rods; Welding Torch Tips; Hardware

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 5050
Tensile Strength 310 MPa45000 psi
Tensile Strength, Yield 82.7 MPa12000 psi0.5% Ext
Tensile Modulus 110 GPa16000 ksi
Modulus of Rigidity 41.4 GPa6000 ksi
Poissons Ratio 0.330.33Calculated
Machinability 75 %75 %
Forgeability 65 %65 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000310 ohm-cm0.00000310 ohm-cm55% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 20.9 W/m-K145 BTU-in/hr-ft²-°F
Melting Point 1040 - 1080 °C1900 - 1980 °F
Solidus 1040 °C1900 °F
Liquidus 1080 °C1980 °F
Annealing Point 482 - 704 °C900 - 1300 °F
 
Processing PropertiesMetricEnglishComments
Solution Temperature 704 - 788 °C1300 - 1450 °F
Hot-Working Temperature 760 - 871 °C1400 - 1600 °F
Precipitation Temperature 454 °C850 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 97 - 98.6 %97 - 98.6 %As Balance
Iron, Fe <= 0.20 %<= 0.20 %
Lead, Pb <= 0.10 %<= 0.10 %
Nickel, Ni 0.90 - 1.3 %0.90 - 1.3 %
Phosphorus, P 0.15 - 0.35 %0.15 - 0.35 %
Tellurium, Te 0.35 - 0.60 %0.35 - 0.60 %
Zinc, Zn <= 0.50 %<= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC19100x2 / 292877

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.