MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Sciengy PPS-SGC501LFRT PPS, 50% Long Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 50% Carbon Fiber Filler

Material Notes: PPS-SGC501LFRT is a 50% long CF reinforced linear polyphenylene sulfide.

Information provided by Shandong Sciengy New Materials Co. Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.54 g/cc0.0556 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 150 MPa21800 psiISO 527-2/1A
Elongation at Break 0.40 %0.40 %ISO 527-2/1A
Tensile Modulus 42.0 GPa6090 ksiISO 527-2/1A
Flexural Strength 340 MPa49300 psiISO 178
Flexural Modulus 39.0 GPa5660 ksiISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²ISO 180A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 280 °C536 °FISO 75-1/-2
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Melt Temperature 285 - 345 °C545 - 653 °FInjection molding; ISO 294
Mold Temperature 140 - 160 °C284 - 320 °FInjection molding; ISO 294
Drying Temperature  120 °C
@Time 18000 sec
248 °F
@Time 5.00 hour
 150 °C
@Time 10800 sec
302 °F
@Time 3.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCIE053 / 297100

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.