MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CIMBAR CIMTUFF® 9110 Talc
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® 9100 Series talcs are primarily used in performance polypropylene, where improved tensile strength, flexural modulus, heat distortion temperature, increased stiffness, reduced shrinkage and lower compounding costs are required. CIMTUFF® 9100 Series talcs are platy, hydrophobic, non-abrasive and chemically inert.

Information provided by Cimbar Performance Minerals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.78 g/cc
Bulk Density 28.0 lb/ft³Loose
 68.0 lb/ft³Tapped
Brightness 90 %Hunter Rd, dry
Oil Absorption 24 %g oil/100 g filler; ASTM D281
Moisture Absorption at Equilibrium 0.30 %
Loss On Ignition 7.5 %
Particle Size 10 µmMedian; Micrometrics Sedigraph 5100
Particle Mesh Size 325 Mesh1.0% retained
pH 8.7
 
Component Elements PropertiesOriginal ValueComments
Al2O3 <= 1.0 %
CaO <= 1.0 %
Fe2O3 <= 1.0 %
MgO 30 %
SiO2 60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CIMBAR CIMTUFF® 9107 Talc
CIMBAR CIMTUFF® 9103 Talc
CIMBAR CIMTUFF® 9102 Talc
CIMBAR RP 9405 Talc
CIMBAR EliteTalc® 21 Cosmetic Talc

CIMBAR938 / 133420

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.