MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kolon KompoGTe® LE1G30HSBL Polypropylene with Glass Fiber + Bead Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with Glass Fiber + Bead Filler

Material Notes: PP LFT +GF 20% + GB 10%

KompoGTe® LFT is produced by impregnation of long fibers into thermoplastics. This provides superior properties compared with short fiber reinforced thermoplastic. Also, it enables production of parts with a higher content of fibers. It is used to replace metal for many industries, such as automotive, electricity & electronics, and other applications. KompoGTe® LFT has homogenized fiber dispersion and excellent impregnation which can lead to superior surface properties and mechanical strength. Processed by injection molding.

Information provided by Kolon Plastic, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 92.0 MPa
@Thickness 3.20 mm
50 mm/min; ASTM D638
Flexural Strength 138 MPa
@Thickness 6.40 mm
10 mm/min; ASTM D790
Flexural Modulus 5800 MPa
@Thickness 6.40 mm
10 mm/min; ASTM D790
Izod Impact, Notched 150 J/m
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 163 °C20°C/min; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 159 °CASTM D648
Flammability, UL94 HB
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 200 - 220 °C
Middle Barrel Temperature 220 - 240 °C
Front Barrel Temperature 230 - 250 °C
Nozzle Temperature 230 - 250 °C
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 80.0 - 90.0 °C
@Time 7200 - 14400 sec
Dehumidifying Dryer
Moisture Content <= 0.10 %
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKOKZ765 / 255776

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.