MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 2208 Water White High Temperature Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2208 is a clear, almost water-white low viscosity epoxy adhesive system recommended for rigid laminating, filament winding, potting and bonding applications. This all-liquid formulation contains no solvents, and is easily mixed, handled and applied at room temperature as it has a very long useful pot-life, however a final elevated temperature bake is REQUIRED for complete cure. TRA-BOND 2208 develops rigid high-strength bonds with excellent mechanical, structural and electrical properties coupled with good color stability, moderate heat resistance and good shock resistance. It adheres to metals, glass, glass products and fabrics, ceramics, rigid plastics and other high-temperature resistant materials. Fully cured TRA-BOND 2208 has superior electrical properties, and it provides excellent resistance to water, weather, vapors, gases and petroleum fuels and lubricants, salt solutions, most mild acids and alkalis, and many other chemical compounds. An additional post-cure of 4 hours at 145°C is recommended when application temperatures higher than 145°C are anticipated.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccMixed
Solids Content 100 %Reactive Solids Content
Viscosity 1030 cP
@Temperature 25.0 °C
After mixing
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87
Tensile Strength, Yield 8700 psi
Elongation at Yield 5.0 %
Izod Impact, Notched 0.290 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.30e+15 ohm-cm
 1.40e+12 ohm-cm
@Temperature 150 °C
Dielectric Constant 3.2
@Frequency 1000 Hz
Dielectric Strength 395 V/mil
Dissipation Factor 0.010
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 175 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 6.00 hour2 hrs @ 65°C + 4 hrs @ 130°C
 10.0 hour2 hrs @ 65°C + 8 hrs @ 115°C
Pot Life 7200 min(5 days)
 
Descriptive Properties
Color Clear
Mix Ratio, parts by weight100/3Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAC059 / 70987

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.