MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

LATI Larton GCE/650 PPS, Glass/Mineral Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

Material Notes: Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.97 g/cc0.0712 lb/in³
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0015 - 0.0030 cm/cm0.0015 - 0.0030 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  90.0 MPa
@Temperature 150 °C
13100 psi
@Temperature 302 °F
 105 MPa
@Temperature 120 °C
15200 psi
@Temperature 248 °F
 125 MPa
@Temperature 90.0 °C
18100 psi
@Temperature 194 °F
 145 MPa
@Temperature 60.0 °C
21000 psi
@Temperature 140 °F
 165 MPa
@Temperature 23.0 °C
23900 psi
@Temperature 73.4 °F
Elongation at Break  0.80 %
@Temperature 23.0 °C
0.80 %
@Temperature 73.4 °F
 0.90 %
@Temperature 60.0 °C
0.90 %
@Temperature 140 °F
 1.0 %
@Temperature 90.0 °C
1.0 %
@Temperature 194 °F
 1.6 %
@Temperature 120 °C
1.6 %
@Temperature 248 °F
 2.3 %
@Temperature 150 °C
2.3 %
@Temperature 302 °F
Tensile Modulus  9.40 GPa
@Temperature 150 °C
1360 ksi
@Temperature 302 °F
 14.2 GPa
@Temperature 120 °C
2060 ksi
@Temperature 248 °F
 20.8 GPa
@Temperature 90.0 °C
3020 ksi
@Temperature 194 °F
 22.0 GPa
@Temperature 60.0 °C
3190 ksi
@Temperature 140 °F
 23.0 GPa
@Temperature 23.0 °C
3340 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 1.50 J/cm²7.14 ft-lb/in²
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 150 V150 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 225 °C437 °F
Deflection Temperature at 0.46 MPa (66 psi) 285 °C545 °F
Deflection Temperature at 1.8 MPa (264 psi) 275 °C527 °F
Vicat Softening Point 260 °C
@Load 5.00 kg
500 °F
@Load 11.0 lb
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
Oxygen Index 45 %45 %
Glow Wire Test  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
GWFI/GWT
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
GWFI/GWT
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 - 330 °C554 - 626 °F
Mold Temperature 130 - 140 °C266 - 284 °F
Drying Temperature 130 - 150 °C
@Time 10800 sec
266 - 302 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
Mitsubishi Chemical Advanced Materials Techtron™ PSBG PPS, Polyphenylene sulfide, bearing grade, compression molded
Lehvoss LUVOCOM® 1301/XCF/30/EG PPS, linear with carbon fiber
Lehvoss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear with carbon fiber, glass fiber and micro glass spheres
Ensinger TECATRON™ PVX Polyphenylene sulfide (PPS), Bearing Grade

PLATH9652 / 177348

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.