HyperCarb can be used as a cost effective alternative to other fine white carbonate products. Applications: - Plastics
- Can be used as a titanium dioxide replacement in plastic masterbatch, it does not impart a yellow hue and is neutral in color. In rigid PVC it gives high brightness values such as those required for window and general purpose.
|