MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE EE-1255 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink EE-1255 is a general purpose thermoplastic elastomer used in automotive applications, including exterior. Sarlink EE-1255 is a medium hardness, high density, lubricated grade exhibiting good Colorability and processability. This grade can be processed by injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Filled; General Purpose; Good Melt Strength; Good Mold Release; Good Processability; Good Processing Stability; High Density; High Specific Gravity; Low Flow; Medium Hardness; Lubricated; Slip

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Automotive Interior Trim

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccISO 1183
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 54
@Time 15.0 sec
Injection Molded; ISO 868
 55
@Time 5.00 sec
Injection Molded; ISO 868
 57
@Time 1.00 sec
Injection Molded; ISO 868
 53.5
@Treatment Temp. 125 °C,
Time 15.0 sec
Change in Air, 168 hr; ISO 888
 55.5
@Treatment Temp. 110 °C,
Time 15.0 sec
Change in Air, 1008 hr; ISO 888
 55.6
@Treatment Temp. 125 °C,
Time 5.00 sec
Change in Air, 168 hr; ISO 888
 57.2
@Treatment Temp. 110 °C,
Time 5.00 sec
Change in Air, 1008 hr; ISO 888
 57.9
@Treatment Temp. 125 °C,
Time 1.00 sec
Change in Air, 168 hr; ISO 888
 59.1
@Treatment Temp. 110 °C,
Time 1.00 sec
Change in Air, 1008 hr; ISO 888
Tensile Strength at Break 421 psiFlow, Type 1, 20 in/min; ISO 37
 812 psiAcross Flow, Type 1, 20 in/min; ISO 37
 435 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 450 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 841 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 884 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain 152 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 328 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 155 psi
@Strain 100 %,
Treatment Temp. 125 °C
Across Flow, Type 1, Change in Air, 168 hr; ISO 188
 162 psi
@Strain 100 %,
Treatment Temp. 110 °C
Across Flow, Type 1, Change in Air, 1008 hr; ISO 188
 348 psi
@Strain 100 %,
Treatment Temp. 110 °C
Flow, Type 1, Change in Air, 1008 hr; ISO 188
 351 psi
@Strain 100 %,
Treatment Temp. 125 °C
Flow, Type 1, Change in Air, 168 hr; ISO 188
Elongation at Break 350 %Flow, Type 1, 20 in/min; ISO 37
 780 %Across Flow, Type 1, 20 in/min; ISO 37
 362 %
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 399 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 801 %
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 832 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
Tear Strength 100 pliAcross Flow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34
 120 pliFlow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34
Compression Set 16 %
@Temperature 22.8 °C,
Time 79200 sec
ISO 815
 36 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 58 %
@Temperature 90.0 °C,
Time 252000 sec
ISO 815
 70 %
@Temperature 125 °C,
Time 252000 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Processing Temperature 440 - 480 °FMelt, Injection
Rear Barrel Temperature 440 - 480 °FInjection
Middle Barrel Temperature 440 - 480 °FInjection
Front Barrel Temperature 440 - 480 °FInjection
Nozzle Temperature 440 - 480 °FInjection
Zone 1 420 - 460 °FExtrusion
Zone 2 420 - 460 °FExtrusion
Zone 3 420 - 460 °FExtrusion
Zone 4 420 - 460 °FExtrusion
Zone 5 420 - 460 °FExtrusion
Die Temperature 420 - 460 °FExtrusion
Mold Temperature 60.0 - 90.0 °FInjection
Injection Pressure 200 - 1000 psiInjection
Back Pressure 25.0 - 125 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Colors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE)
Teknor Apex Sarlink® TPE OM-1150N Thermoplastic Elastomer
Teknor Apex Sarlink® TPE ML-1650N NAT Thermoplastic Elastomer
Teknor Apex Sarlink® TPE ML-1150N NAT Thermoplastic Elastomer
Teknor Apex Sarlink® TPE ME-2350B BLK Thermoplastic Elastomer

PTEKNQ1022 / 237513

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.