ISO data as provided by the manufacturer, Creanova, Inc. Glass fiber reinforced (12%), self-extinguishing PBT resin in accordance with UL 94 with non-migrating flame retardants and enhanced rigidity. This former Creanova product line is a part of Degussa AG as of 2001. This grade is not part of the current Degussa product line. |