Notes: Monprene IN-22215 XRD1 is a general purpose thermoplastic elastomer, available in NAT and colors, designed for a variety of industrial applications, including seals and gaskets. Monprene IN-22215 XRD1 is a low density, low hardness, RoHS compliant grade that is suitable for injection molding and extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Abrasion Resistant; Chemical Resistant; Foamable; Good Adhesion; Good Colorability; Good Moldability; Good Processability; Good Processing Stability; Halogen Free; High Elongation; High Flow; Low Density; Low Hardness; Low Specific Gravity; Without Fillers Uses: Foam; Gaskets; Handles; Hose; Industrial Applications; Low Temperature Applications; Pipe Seals; Profiles; Rubber Replacement; Seals; Tubing; Windows & Doors RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Preliminary data. Information provided by Teknor Apex |