MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Durethan® BKV 130 H3.0 101006 Copolyamide, 30% Glass Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30 H3.0, even in the dry state, good heat-ageing resistance

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183
Water Absorption 7.0 %Test Sim. to ISO 62
Moisture Absorption at Equilibrium 2.0 %23°C/50% R.H.; Test Sim. to ISO 62
Viscosity Number 134 cm³/gISO 307, 1157, 1628
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 260 °C
Estimated using room temperature density; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 100 MPaConditioned; ISO 527-1/-2
 160 MPaISO 527-1/-2
Elongation at Break 4.0 %ISO 527-1/-2
 7.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 5200 MPaConditioned; ISO 527-1/-2
 9000 MPaISO 527-1/-2
Charpy Impact Unnotched 80.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 80.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 95.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 110 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 18.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 28.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
Puncture Energy 10.0 JISO 6603-2
 15.0 JConditioned; ISO 6603-2
 7.00 J
@Temperature -30.0 °C
ISO 6603-2
 7.00 J
@Temperature -30.0 °C
Conditioned; ISO 6603-2
Tensile Creep Modulus, 1 hour 4200 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 3300 MPaISO 899-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°CISO 11359-1/-2
Melting Point 213 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 90.0 °CISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
Oxygen Index 22 %ISO 4589-1/-2
 
Descriptive Properties
FeaturesHeat stabilized or stable to heat
 High impact or high impact modified
FormPellets
ISO Short NameISO 1874-PA 6/66-I, MHR, 14-090, GF30
ProcessingInjection molding
RegionAsia Pacific
 Europe
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Durethan® BKV 130 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Dry
Overview of materials for Polyester Thermoplastic Elastomer
Overview of materials for Polyether Block Amide (PEBA)
Envalior Durethan® BKV 30 H2.0 EF 900116 Nylon 6, 30% Glass Fiber
Envalior Durethan® A 30 S FN31 000000 Nylon 66 (PA66), Dry

PLANX0746 / 98961

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.