MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Accella Bayseal® 3.0 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Characterization: Bayseal 3.0 is a two-component, closed-cell spray-applied polyurethane foam (SPF) system.

Properties / Applications: Bayseal 3.0 SPF offers high compressive strengths, smooth aesthetics and a broad application temperature window. The Bayseal 3.0 system is self flashing and provides protection by helping to seal cracks, crevices and holes while insulating decks from temperature extremes. The Bayseal 3.0 spray polyurethane foam system comprises an "A" component, which is a polymeric diisocyanate, and a "B" component, which is a combination of polyols, additives, and HFC-245fa blowing agent. As with any product, use of Bayseal 3.0 foam-forming system must be tested (including, but not limited to, field testing) in advance by the user to determine suitability.

Covestro sold their spray polyurethane foam business to Accella in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.0481 g/cc0.0481 g/ccCore Density
Water Absorption <= 2.0 %<= 2.0 %ASTM D2842
Viscosity 150 - 250 cP150 - 250 cPComponent A
 500 - 650 cP500 - 650 cPComponent B
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 0.621 MPa90.1 psiASTM D1623
Compressive Strength 0.345 MPa50.0 psiASTM D1621
 
Thermal PropertiesMetricEnglishComments
Insulation R Value  6.4
@Thickness 25.4 mm
6.4
@Thickness 1.00 in
aged; ASTM C518
 23.5
@Thickness 88.9 mm
23.5
@Thickness 3.50 in
aged; ASTM C518

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BCC Products MB 1200 Polyurethane Foam Modeling Board
Covestro Baynat® 3002 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-3818 FST Polyurethane Foam
General Plastics LAST-A-FOAM® FR-6718 Polyurethane Foam
Accella Bayseal® 2.7 Polyurethane

PCOVEST0224 / 202007

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.