MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK Laponite® RDS Synthetic Layered Silicate
Categories: Ceramic; Clay

Material Notes: Description: Laponite RDS is a synthetic layered silicate incorporating an inorganic polyphosphate peptiser. It hydrates and swells in water to give clear and colourless colloidal dispersions of low viscosity known as sols. At 10% concentration in water, these will remain free flowing for 24 hours. On addition of small quantities of electrolyte, highly thixotropic gels are formed rapidly.

Application: Laponite RDS may be utilized as a predispersed liquid concentrate and added to formulations at any point during manufacture. It is used to impart a shear sensitive structure to a wide range of waterborne formulations including household and industrial surface coatings, cleansers, agrochemical and horticultural products. Laponite RDS may be coated onto paper or other surfaces from concentrated sols to give smooth, coherent, and electrically conductive films.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 62.4 lb/ft³
Particle Mesh Size >= 250 Mesh<2%
pH 9.72% suspension
Specific Surface Area 330 m²/g
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 10 %Free
Loss on Ignition(%) 8.0 %
MgO 26 %
Na2O 5.6 %
P2O5 4.4 %
SiO2 54.5 %
 
Descriptive Properties
Color/FormFree flowing white powder
Composition0.008Li2O

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Laponite® JS Clay Additive
BYK Laponite® RD Synthetic Layered Silicate
BYK Cloisite® 10A Nanoclay
BYK Laponite® SL25 Thickener
BYK Laponite® S Synthetic Layered Fluorosilicate

PBYK067 / 185064

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.