MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PSM Industries Pacific Sintered Metals FCC-216-P High Carbon Copper Steel Powdered Metal (MPIF FC-0208-40)
Categories: Metal; Ferrous Metal; Carbon Steel; High Carbon Steel

Material Notes: High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.

Equivalent MPIF Specification: FC-0208-40

All information provided by Pacific Sintered Metals.

Key Words: PM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.00 - 6.40 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 61
Tensile Strength, Ultimate 50000 psi
Tensile Strength, Yield 45000 psi
Elongation at Break <= 1.0 %
Flexural Strength 90000 psiTransverse Rupture
Bearing Yield Strength 49000 psi
Charpy Impact, Unnotched 2.00 ft-lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PSM Industries Pacific Sintered Metals FCC-214-S High Carbon Copper Steel Powdered Metal (MPIF FC-0208-50)
PSM Industries Pacific Sintered Metals FCC-216-P(HT) High Carbon Copper Steel Powdered Metal (MPIF FC-0208-50HT)
PSM Industries Pacific Sintered Metals FCC-214-S(HT) High Carbon Copper Steel Powdered Metal (MPIF FC-0208-80HT)
PSM Industries Pacific Sintered Metals FN-255-S(HT) Nickel Steel Powdered Metal (MPIF FN-0208-130HT)
PSM Industries Pacific Sintered Metals FCC-200-P High Carbon Copper Steel Powdered Metal (MPIF FC-0505-40)

NPACIF011 / 86169

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.