MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Reynolds EZ~Spray® StyroCoat® Flame Rated Sprayable Plastic Coating
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: StyroCoat® Plastic is a flame rated (E-84) sprayable polyurethane plastic formulated to economically coat a variety of surfaces. Dispensed through Smooth-On’s EZ~Spray®, Jr. cartridge system, the plastic cures in about 2 seconds and can be applied to vertical surfaces without running off. An advantage of the system is that large areas can be covered in a short period of time. Cured plastic is lightweight, flame, impact, and water resistant. It can be sanded for priming and painting. Plastic can also be sprayed into a rubber mold to make fast, impact resistant castings (application of a release agent may be necessary before spraying into the mold). StyroCoat® Plastic is used for theme design / fabrication applications, making movie set environments, making surfaces water resistant and other industrial applications.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D-1475
Linear Mold Shrinkage 0.015 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ASTM D-2240
Tensile Strength, Ultimate 3170 psiASTM D-638
Elongation at Break 20 %ASTM D-638
Tensile Modulus 131000 psiASTM D-638
Flexural Strength 6400 psiASTM D-790
Flexural Modulus 205000 psiASTM D-790
Compressive Strength 5000 psiASTM D-695
Compressive Modulus 47600 psiASTM D-695
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 minHandling Time
Pot Life 0.0330 minASTM D-2471
 
Descriptive Properties
ColorOff-White
Mix Ratio1A:1B pbvby volume
Mixed ViscosityVariable
Specific Volume24.7[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN053 / 296754

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.