Diamaloy GLY 9020 resin is a high-gloss, low impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it can be easily coextruded. This product is supplied in various colors. Applications: Typical applications include those requiring weatherability and high gloss such as body panels for tractors, recreational vehicles, etc. As with any product, use of Diamaloy GLY 9020 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. A. Schulman has acquired Network Polymers & Diamond Polymers. |