MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel CLC 18.10 L General Purpose 18Cr-10Ni Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T S30000 Series Stainless Steel

Material Notes: Description: CLC 18-10L is a 18Cr-10Ni austenitic stainless steel. The grade contains small amount of ferrite (~ 3%) after solution annealing (1000-1100°C – 1832-2012°F) and water quenching. This kind of steel is one of the basic grades of the stainless steels range. Its low carbon content ensures better ductility and avoids the intergranular corrosion, even on welded pieces without ulterior water quenching. Alloys CLC 18-10L exhibits an austenitic microstructures free of deleterious carbide precipitations at grain boundaries. The main properties of CLC 18-10L are: basic corrosion resistance, resistance against intergranular corrosion, and high ductility.

Tensile properties after water quenching.

Information provided by manufacturer.

Key Words: EURONORM 1.4306 X2CrNi18-11, AFNOR Z3 CN 18-10, DIN W1.4306, ASTM A 240 – TP 304L, UNS S30403
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 570 MPaTypical
 520 - 650 MPaMinimum Guaranteed
Tensile Strength, Yield >= 200 MPa
@Strain 0.2 %
 >= 240 MPa
@Strain 1 %
 265 MPa
@Strain 0.2 %
Typical
 305 MPa
@Strain 1 %
Typical
Elongation at Break 45 %
Modulus of Elasticity 200 GPa
@Temperature 20.0 - 100 °C
Poissons Ratio 0.299Calculated
Shear Modulus 77.0 GPa
@Temperature 20.0 - 100 °C
Charpy Impact >= 185 J
 310 JTypical
 >= 125 J
@Temperature -196 °C
 250 J
@Temperature -196 °C
Typical
Charpy Impact, Unnotched 158 J
@Temperature 200 °C
Transverse
 265 J
@Temperature 200 °C
Longitudinal
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000730 ohm-cm
@Temperature 20.0 - 100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 - 100 °C
 17.0 µm/m-°C
@Temperature 20.0 - 300 °C
 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
 18.0 µm/m-°C
@Temperature 20.0 - 500 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 15.0 W/m-K
@Temperature 20.0 - 100 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.020 %
Chromium, Cr 18.5 %
Iron, Fe 71.23 %As remainder
Nickel, Ni 10.2 %
Nitrogen, N 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel
Industeel CLC 18.9 L General Purpose 18Cr-9Ni Austenitic Stainless Steel
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel
AISI Type 304L Stainless Steel
Outokumpu 4404 Cr-Ni-Mo Austenitic Stainless Steel

NINDUST02 / 17540

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.