MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ovako 19MnV6* 280T Steel, +AR
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Ovako 280T is a premium variant used in the hollow bar program of Ovako. Ovako 280T meet and is exceeding the demands of E470 in EN10294-1. Ovako 280T is a micro alloyed steel with high tensile strength, good machinability and weldability.
  • Suitable for case carburizing or nitriding
  • Good dimensional stability
  • Fine-grain treated
  • Delivered in as-rolled, normalized or quenched and tempered condition
  • Weldable if preheated
Information provided by Ovako
Key Words: 19MnVS6, E470, 20MnV6, 20 MV 6, SS 2142, 1.1301, 19MnV6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 200
@Thickness 24.0 - 190 mm
Round bar
 200
@Thickness 24.0 - 190 mm
Round bar
 220
@Thickness >=25.0 mm
Tube, wall
 225
@Thickness <=25.0 mm
Tube, wall
Tensile Strength 550 MPa
@Thickness 24.0 - 190 mm
Round bar
 620 MPa
@Thickness 24.0 - 190 mm
Round bar
 640 MPa
@Thickness >=25.0 mm
Tube, wall
 670 MPa
@Thickness <=25.0 mm
Tube, wall
Tensile Strength, Yield >= 410 MPa
@Thickness 24.0 - 190 mm
Reh, Round bar
 >= 450 MPa
@Thickness 24.0 - 190 mm
Reh, Round bar
 >= 470 MPa
@Thickness >=25.0 mm
Reh, Tube, wall
 >= 500 MPa
@Thickness <=25.0 mm
Reh, Tube, wall
Elongation at Break 19 %
@Thickness 24.0 - 190 mm
Round bar
 20 %
@Thickness <=25.0 mm
Tube, wall
 20 %
@Thickness >=25.0 mm
Tube, wall
 20 %
@Thickness 24.0 - 190 mm
Round bar
Modulus of Elasticity 210 GPa
Poissons Ratio 0.30
Shear Modulus 80.0 GPa
Impact Test 27.0 J
@Thickness 24.0 - 190 mm,
Temperature 20.0 °C
Round bar, long
 27.0 J
@Thickness 24.0 - 190 mm,
Temperature 20.0 °C
Round bar, long
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.460 - 0.480 J/g-°C
@Temperature 50.0 - 100 °C
Thermal Conductivity 40.0 - 45.0 W/m-KAmbient temperature
Transformation Temperature 395 °CMS
 721 °CAC1
 810 °CAC3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.17 - 0.20 %
Chromium, Cr 0.20 - 0.28 %
Iron, Fe 96.99 - 97.78 %As Balance
Manganese, Mn 1.45 - 1.6 %
Molybdenum, Mo <= 0.10 %
Nickel, Ni <= 0.20 %
Phosphorus, P <= 0.025 %
Silicon, Si 0.30 - 0.45 %
Sulfur, S 0.020 - 0.035 %
Vanadium, V 0.080 - 0.12 %
 
Descriptive Properties
Dl1.6-1.9%
WeldabilityCEV 0.6max
 Pcm 0.35max

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Type AL 441HP™ Stainless Steel Alloy
ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035)
ATI Allegheny Ludlum AL 433™ Ferritic Stainless Steel, Annealed
Astralloy 4800® Wear Resistant Steel
ASTM A542/A542M Alloy Steel, Chromium Molybdenum

NOVAKO111 / 234410

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.