MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: Description: Injection Molding, PC, Halogen Free Flame Retardant, High Heat Resistance

Application: IT/OA Housing and Components (Adaptor)

CAS: 103598-77-2

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Maximum Moisture Content 0.020Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 12 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength, Yield 630 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break >= 100 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Flexural Yield Strength 970 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Flexural Modulus 23000 kg(f)/cm²
@Thickness 3.20 mm
10mm/min; ASTM D790
Izod Impact, Notched >= 77.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 175 - 250 V
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Vicat Softening Point 140 °C
@Load 5.00 kg
50°C/h; ASTM D1525
UL RTI, Electrical 80.0 °C
@Thickness >=1.00 mm
 120 °C
@Thickness >=1.50 mm
 120 °C
@Thickness >=1.70 mm
 125 °C
@Thickness >=3.00 mm
UL RTI, Mechanical with Impact 80.0 °C
@Thickness >=1.00 mm
 115 °C
@Thickness >=1.50 mm
 115 °C
@Thickness >=1.70 mm
 120 °C
@Thickness >=3.00 mm
UL RTI, Mechanical without Impact 80.0 °C
@Thickness >=1.00 mm
 120 °C
@Thickness >=1.50 mm
 120 °C
@Thickness >=1.70 mm
 125 °C
@Thickness >=3.00 mm
Flammability, UL94 V-0
@Thickness >=1.00 mm
 V-0
@Thickness >=1.50 mm
 V-0
@Thickness >=1.70 mm
 V-0
@Thickness >=3.00 mm
 5VB
@Thickness >=3.00 mm
 5VA
@Thickness >=1.70 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 280 °CInjection Molding
Middle Barrel Temperature 280 - 300 °CInjection Molding
Front Barrel Temperature 300 - 320 °CInjection Molding
Nozzle Temperature 300 - 320 °CInjection Molding
Melt Temperature 300 - 320 °CInjection Molding
Mold Temperature 80.0 - 120 °CInjection Molding
Drying Temperature 100 - 120 °CInjection Molding
Dry Time 3.00 - 5.00 hourInjection Molding
Back Pressure 0.981 - 3.92 MPaInjection Molding
Screw Speed 40 - 70 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUPOY GP1006FM PC, Flame Retardant
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance
LG Chemical LUPOY GP1000MD PC, Light Diffusion
LG Chemical LUPOY GP1006FL PC, Flame Retardant

PLAY540 / 148550

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.